cooling speed Application: refrigeration parts Raw materials (Al plate)1.Al plate: the thickness of finished product is 1.1-2.0mm2.the thickness of raw Al plate:1.7-2.15mm key process:preparing materials – cleaning – printing – rolling – annealing - blowing up – punching –folding and sharpening –add the capillary – assemble welding – leakage testing – cleaning and drying – coating - inspection – packing.Max dimension: width 600mm, length 1500mm.We can produce according to your requirement. Structure:Double side roll bond evaporatorSingle side roll bond evaporatorPart single side roll bond evaporator. Performance:Surface is treated with powder painting to prevent the corrosion.Inner cleanness can meet the requirement of R134a&CFC cooling system.Can satisfy the cooling capability.
showcase&a/c parts(heat exchanger)